I bumped the nozzle temp another 5 degrees and I think it’s pretty good now. I should do a temp tower tbh but I got toys to print.
Left is 260c middle is 255c and right is a completely different model at 255c. Hardened steel nozzle with PETG.
The difference between the top infills is staggering. I was experimenting for strength but they look so bad I’m not gonna consider them for the top. On the bottom the bed seems to melt them in a bit and smooth them out.